Fig. 3: Nanomechanical and Raman vibrations measured from the 3 L WSe2 resonator with d = 4 μm, using Vg = 3 V, and vac from 30 mV to 200 mV (Full data with vac from 5 mV to 200 mV are shown in Fig. S10).

a Select amplitude-frequency curves showing nanomechanical responses under different vac. The insets in (a) show vibrational amplitude of WSe2 membrane as a function of vac at 11.02 MHz. b Select Raman spectra with the device driven at driving frequency 11.02 MHz, Vg = 3 V, showing E2g1 & A1g and 2LA modes, when vac = 200 mV (red, device in nonlinear regime) and vac = 10 mV (blue, device in linear regime). Symbols are measured spectra data and dashed lines are fittings to the individual peaks, with solid lines being the sums. The insets in (b) show Raman peak shift ∆ωE2g1& A1g (left) and ∆ω2LA (right) as a function of vac at 11.02 MHz (indicated by colored triangles). The measurement conditions in (b) largely correspond to the symbols in (a)