Fig. 1: OER activity of Co2FeO4 and CoFe2O4 nanoparticles.
From: 3D atomic-scale imaging of mixed Co-Fe spinel oxide nanoparticles during oxygen evolution reaction

a, b Linear sweep voltammetry (LSV) curves recorded at a scan rate of 10 mV/s in 1.0 M KOH on glassy carbon electrodes deposited with Co2FeO4 and CoFe2O4 nanoparticles in the pristine state and after 100, 500 and 1000 cycles of cyclic voltammetry (CV) measurements, c, d CVs of Co2FeO4 and CoFe2O4 after one, 100, 500 and 1000 cycles recorded at a scan rate of 50 mV/s in 1.0 M KOH under OER conditions, e, f Tafel slopes of Co2FeO4 and CoFe2O4 in the pristine and after 100, 500 and 1000 cycles, derived from the LSV curves in a, b. Source data are provided as a Source Data file. The error bars of Tafel slopes in e, f were measured by linear curve fitting.