Fig. 5: Schmid factor (SF) distributions and the total elongation-<110 > //RD relations for A-1200 and B-1200.
From: Revealing the room temperature superplasticity in bulk recrystallized molybdenum

a–d The average SF of A-1200 and B-1200 are 0.469 and 0.459 respectively, which are higher than 0.45. e–f The texture components and total elongation of samples A and B annealed at 1000 °C, 1100 °C, 1200 °C and 1700 °C. The ratios of <110> //RD texture in annealed samples A and B are different (Fig. 1b, c and Supplementary Figs. 12–14), and their respective total elongations did not show a simple linearity with the variation of texture ratio for B samples.