Extended Data Fig. 4: SEM and elemental mapping of S and S9.3I mixed with LPS after heating at 100 °C. | Nature

Extended Data Fig. 4: SEM and elemental mapping of S and S9.3I mixed with LPS after heating at 100 °C.

From: Healable and conductive sulfur iodide for solid-state Li–S batteries

Extended Data Fig. 4

The SEM image of S/LPS mixture (a) and S9.3I/LPS mixture (b) after milling and heating at 100 °C. (c) The cross sectional cryo-FIB SEM images and corresponding element distribution images of S/LPS for S and P. The distribution of S and P is inhomogeneous. (d) Distribution of S, P, and I in S9.3I/LPS. The distribution in the entire area is homogeneous.

Back to article page