Figure 3
From: High-purity recycling of hematite and Zn/Cu mixture from waste smelting slag

SEM images of the precipitated particles generated at molar ratios of (A) 0, (B) 0.5, (C) 1 and (D) 2.
From: High-purity recycling of hematite and Zn/Cu mixture from waste smelting slag
SEM images of the precipitated particles generated at molar ratios of (A) 0, (B) 0.5, (C) 1 and (D) 2.