Figure 9
From: Centrifugal granulation behavior in metallic powder fabrication by plasma rotating electrode process

Morphology of the Ti64 electrode end surface after PREP under the operating conditions corresponding to the cases in Fig. 5 with gas flow rates of (a) 0, (b) 70, and (c) 160 L/min.