Figure 1
From: Origin of perpendicular magnetic anisotropy in amorphous thin films

(a) The XRD spectrum of Co–Zr–Ta–B films deposited under different argon sputtering pressures (1.6–6.2 mTorr). (b) SAED pattern of the film deposited under 6.2 mTorr argon pressure.