Fig. 1

(a) Schematic of the optothermal Raman experiment setup for the strained MoS2 monolayer. (b) Morphology of the MoS2 monolayer prior to tensile strain captured using an optical microscope. (c) Morphology of the MoS2 monolayer subjected to the tensile strain of 6.3% captured using the optical microscope.