Fig. 8: Depth analysis elements within corrosion film on Mg-Nd-Zr alloys. | npj Materials Degradation

Fig. 8: Depth analysis elements within corrosion film on Mg-Nd-Zr alloys.

From: Attain insensitivity to chlorine ions in magnesium alloys by impeding the diffusion process

Fig. 8

a AES depth analysis of total elements in Mg in 3.5 wt.% NaCl solution. b AES depth analysis of total elements in Mg in 10 wt.% NaCl solution. c AES depth analysis of total elements in Mg in 3.5 wt.% NaCl solution. d AES depth analysis of total elements in Mg in 10 wt.% NaCl solution. e AES spectra of Cl in Mg-Nd-Zr serving in different concentrations NaCl.

Back to article page