Extended Data Fig. 8: Power recovery in light-induced degradation.
From: Flexible silicon solar cells with high power-to-weight ratios

a, VOC, FF, JSC variation of the FT (57 μm) cell during light-induced degradation ageing. b, VOC, FF, JSC variation of the FT (84 μm) cell during light-induced degradation ageing. c, VOC, FF, JSC variation of the SF (125 μm) cell during light-induced degradation ageing. d, VOC, FF, JSC variation of the conventional SHJ (150 μm) cell during light-induced degradation ageing. The dashed lines in the panels are fit lines to evaluate the data change trends.