Figure 4
From: Structural characterisation of high-mobility Cd3As2 films crystallised on SrTiO3

Evolution of crystallinity and transport properties. (a) Annealing temperature dependence of the rocking curve width for the out-of-plane (224) Cd3As2 film peak and the in-plane (4\(\overline{4}\)0) film peak. (b) Same plots for longitudinal conductivity σ xx , carrier density n, and the electron mobility μ at 2 K. (c) Normalised longitudinal magnetoresistance.