Figure 5
From: Centrifugal granulation behavior in metallic powder fabrication by plasma rotating electrode process

(a–c) Ti64 powders and (d, e) corresponding PSD fabricated using an electrode with a diameter of 15 mm, at 11,700 rpm and current of 80 A. The flow rates of argon were (a) 0, (b) 70 and (c) 160 L/min.