Figure 5

(a) Average ligament width in Ni–20Cr foils after corrosion in different molten salt conditions as a function of reaction time at 700 °C. The values for standard deviation of the measurements are also labeled as error bars. (b) Thickness of Ni–20Cr foils versus reaction time after corrosion in different salt conditions as a function of reaction time at 700 °C.