Table 5 Hardness variation.
From: Research on crack propagation behaviour of EB-PVD TBCs based on TGO evolution
H (GPa) | As-received | 25Â h | 50Â h | 75Â h | 25 cycles | 50 cycles |
---|---|---|---|---|---|---|
TC | 10.3719 | 14.1888 | 9.5543 | 10.6410 | 14.2983 | 9.9428 |
TGO | – | 32.9226 | 37.5685 | 20.0772 | 27.4615 | 38.9057 |
BC | 7.6247 | 7.8930 | 6.4323 | 5.8502 | 9.0081 | 6.3914 |