Table 1 Textural properties of the catalysts.

From: Synergistic oxidation of toluene through bimetal/cordierite monolithic catalysts with ozone

Samples

a: Before reaction

b: After reaction without ozone

c: After reaction with ozone

BET surface area (m2/g)

Pore volume (cm3/g)

Average pore diameter (nm)

Cord

a

1.0621

0.0030

11.926

Mn1Co4/Cord

a

6.5071

0.0154

8.6700

b

3.8129

0.0105

10.2760

c

6.7032

0.0160

8.8564

Mn2Co3/Cord

a

10.1179

0.0222

8.5710

b

5.3717

0.0128

9.5392

c

10.1063

0.0220

8.5364

Mn3Co2/Cord

a

7.5485

0.0176

6.5262

b

4.8054

0.0119

9.7304

c

7.4387

0.0173

6.4965

Mn4Co1/Cord

a

9.0851

0.0178

7.6135

b

5.2623

0.0123

9.2196

c

9.0749

0.0179

7.6097