Table 1 The specific surface area, pore volume and average pore size of different samples.
From: Improved surface acidity of CeO2/TiO2 catalyst by Cu doping to enhance the SCR catalytic activity
Samples | Specific surface area (m2/g) | Pore volume (cm3/g) | average pore size (nm) |
---|---|---|---|
CeTi | 86.96 | 0.089 | 4.49 |
CeTiCu0.1 | 116.23 | 0.118 | 4.20 |
CeTiCu0.2 | 119.21 | 0.119 | 3.75 |
CeTiCu0.3 | 130.80 | 0.128 | 3.66 |