Table 3 EDS elemental composition (at%) of the points shown in Fig. 6.
From: Friction stir welding of Haynes 282 Ni superalloy by using a novel hemispherical tool
Analysis point | Ni | Mo | Cr | Ti | Al |
---|---|---|---|---|---|
As-welded | |||||
Ti-Mo rich phase (MC): 1 | 6.54 | 33.22 | 4.66 | 53.25 | - |
Cr-rich phase (M23C6): 2 | 63.19 | 9.15 | 23.53 | 2.49 | 1.61 |
Aged | |||||
Ti-Mo rich phase (MC): 1 | 4.32 | 35.14 | 4.03 | 54.35 | - |
Cr-rich phase (M23C6): 2 | 64.00 | 8.95 | 22.86 | 2.49 | 1.70 |