Table 4 Resilient modulus values for various combinations.
From: Sustainable subgrade improvement with calcium carbide residue and rice husk ash
Sr. No. | Composition | Soaked CBR (%) | Resilient modulus, MPa |
---|---|---|---|
1 | BCS::100 | 1.98 | 19.80 |
2 | BCS: CCR::95:5 | 4.52 | 45.20 |
3 | BCS: CCR::90:10 | 8.56 | 69.55 |
4 | BCS: CCR::85:15 | 8.98 | 71.71 |
5 | BCS: CCR::80:20 | 9.02 | 71.92 |
6 | BCS: CCR::75:25 | 9.15 | 72.58 |
7 | BCS: CCR: RHA::85:10:5 | 9.98 | 76.73 |
8 | BCS: CCR: RHA::80:10:10 | 11.26 | 82.89 |
9 | BCS: CCR: RHA::75:10:15 | 12.4 | 88.17 |
10 | BCS: CCR: RHA::70:10:20 | 12.8 | 89.98 |
11 | BCS: CCR: RHA::65:10:25 | 13.1 | 91.32 |