Fig. 7: Defect distributions in MoTaVW alloy during a radiation damage process.
From: General-purpose machine-learned potential for 16 elemental metals and their alloys

Defect snapshots of a cascade in a MoTaVW alloy at (a) the peak damage state (at about 0.6 ps) and (b) the final damage state (at 140 ps). The red and blue dots represent interstitial atoms and vacancies, respectively. The initial and final molecular dynamics configurations are provided in the Supplementary Data90.