Table 8 Calculation results of Equivalent Compressive Toughness Index.

From: A study on the mechanical and economic performance comparison of ceramsite concrete based on fiber selection and optimization

Specimen group

Deformation

Ω0.85

Ω0.5

Wcu0.85

Growth rate

Wcu0.5

Growth rate

δ0.85

δ0.5

WF-0%

1.081

1.239

110,681

126,811

0.03689

0.0%

0.04227

0.0%

CF-0.6%

1.074

1.158

89,803

99,173

0.02993

-18.9%

0.03306

-21.8%

PF-0.3%

1.068

1.452

105,240

147,300

0.03508

3.2%

0.0491

16.2%

PF-0.6%

1.044

1.133

119,248

129,945

0.04124

11.8%

0.04332

14.3%

PF-0.9%

1.104

1.302

132,840

163,560

0.04428

20.0%

0.05452

29.0%

SF-0.3%

1.180

1.620

144,213

198,370

0.04807

30.3%

0.06612

56.4%

SF-0.6%

1.284

3.12

161,289

425,356

0.05376

45.7%

0.14179

235.4%

SF-0.9%

1.476

3.44

204,827

453,409

0.06828

85.1%

0.15114

257.6%

  1. Note: Each data in the table represents the average of three specimens.